Does anyone know what happened to this?
It featured in MRJ 11, doing nasty things to steel gears and axles, but also quite effectively removing solder from brass parts. It was apparently a strong liquid like Carr's Acidip but even more so - up on the scale of things with cheap calvados and any alcohol produced in a former Soviet state.
Looking on the Carrs (C&L) website now, it seems unavailable.
I have a friend's etched brass kit, or the parts thereof, which is somewhat the worse for wear having been exposed to Powerflow flux and some dodgy soldering. Whilst the worst of the crud has come off with Acidip and several runs in the ultrasonic tank, the solder is in a thin film over much of it.
I could burnish it off with a fibreglass brush, but it will be difficult in some crevices. Also I don't want to apply heat to melt it all off as many parts of the model are correctly soldered together.
So does anyone have a suggestion for this, or a similar product?
Cheers
Flymo
Carrs' Solder Stripper
-
- Forum Team
- Posts: 3046
- Joined: Sun Jul 20, 2008 6:00 pm
Carrs' Solder Stripper
Beware of Trains - occasional modelling in progress!
www.5522models.co.uk
www.5522models.co.uk
-
- Web Team
- Posts: 1231
- Joined: Wed Oct 01, 2008 5:08 pm
Re: Carrs' Solder Stripper
Flymo748 wrote:I have a friend's etched brass kit, or the parts thereof, which is somewhat the worse for wear having been exposed to Powerflow flux and some dodgy soldering.
I have a suspicion that is this: viewtopic.php?f=39&t=1295 (or rather the dismantled remains thereof). If I'm right, thanks Flymo!
I'm looking forward to re-exposing it to my dodgy soldering
-
- Forum Team
- Posts: 3046
- Joined: Sun Jul 20, 2008 6:00 pm
Re: Carrs' Solder Stripper
John McAleely wrote:Flymo748 wrote:I have a friend's etched brass kit, or the parts thereof, which is somewhat the worse for wear having been exposed to Powerflow flux and some dodgy soldering.
I have a suspicion that is this: http://scalefour.org/forum/viewtopic.php?f=39&t=1295 (or rather the dismantled remains thereof). If I'm right, thanks Flymo!
I'm looking forward to re-exposing it to my dodgy soldering
Hi John,
Yes, you're correct - I was trying to keep your name out of the newspapers
It's already come up very nicely, and I'd just like to get some of the solder out of the more inaccessible places...
As for your soldering, it's come on in leaps and bounds since you first did this - you should be very pleased with it! It just shows what jumping in at the deep end can do, with a bit of advice and a lot of practice.
Flymo
Beware of Trains - occasional modelling in progress!
www.5522models.co.uk
www.5522models.co.uk
-
- Posts: 1116
- Joined: Mon Jul 21, 2008 7:39 pm
Re: Carrs' Solder Stripper
Paul,
I once found that the Solder Stripper would not only remove excess solder, it could also dismantle soldered joints. It wasn't very selective in its action.
As solder takes paint better than brass, why not use a liquid flux and spread the excess into a thin film where possible. It can then be more easily removed with a fibreglass brush or simply left.
Jol
I once found that the Solder Stripper would not only remove excess solder, it could also dismantle soldered joints. It wasn't very selective in its action.
As solder takes paint better than brass, why not use a liquid flux and spread the excess into a thin film where possible. It can then be more easily removed with a fibreglass brush or simply left.
Jol
-
- Forum Team
- Posts: 3046
- Joined: Sun Jul 20, 2008 6:00 pm
Re: Carrs' Solder Stripper
John McAleely wrote:Flymo748 wrote:I have a friend's etched brass kit, or the parts thereof, which is somewhat the worse for wear having been exposed to Powerflow flux and some dodgy soldering.
I have a suspicion that is this: http://scalefour.org/forum/viewtopic.php?f=39&t=1295 (or rather the dismantled remains thereof). If I'm right, thanks Flymo!
I'm looking forward to re-exposing it to my dodgy soldering
Here you are then John...
No Solder Stripper involved, just some Acidip to remove the last traces of flux, several turns in the ultrasonic bath, a bit of filing and burnishing, further trips through the bath and it's ready for a rebuild
I'm afraid that the ultrasonic bath also did a good job at vibrating off the more weakly soldered bits, but I think that I have captured all the loose bits!
I'll bring it along to the next CHEAG meeting...
Cheers
Flymo
You do not have the required permissions to view the files attached to this post.
Beware of Trains - occasional modelling in progress!
www.5522models.co.uk
www.5522models.co.uk
-
- Web Team
- Posts: 1231
- Joined: Wed Oct 01, 2008 5:08 pm
Re: Carrs' Solder Stripper
Flymo748 wrote:No Solder Stripper involved, just some Acidip to remove the last traces of flux, several turns in the ultrasonic bath, a bit of filing and burnishing, further trips through the bath and it's ready for a rebuild
That looks great - thank you. This time I should be able to get the sole bars the correct distance apart, and the whole thing rectangular
-
- Forum Team
- Posts: 3046
- Joined: Sun Jul 20, 2008 6:00 pm
Re: Carrs' Solder Stripper
John McAleely wrote:Flymo748 wrote:No Solder Stripper involved, just some Acidip to remove the last traces of flux, several turns in the ultrasonic bath, a bit of filing and burnishing, further trips through the bath and it's ready for a rebuild
That looks great - thank you. This time I should be able to get the sole bars the correct distance apart, and the whole thing rectangular
And to return to this thread, yesterday John brought his rebuilt wagon along to the CHEAG workshop. The photos show that he has made a pretty impressive job from the collection of salvaged parts that I gave back to him...
It's fantastic to see what change can happen in someone's modelling skills in twelve months
Flymo
You do not have the required permissions to view the files attached to this post.
Beware of Trains - occasional modelling in progress!
www.5522models.co.uk
www.5522models.co.uk
-
- Web Team
- Posts: 1231
- Joined: Wed Oct 01, 2008 5:08 pm
Re: Carrs' Solder Stripper
Thank you Paul! I've made more progress today, and the wagon now rolls
-
- Posts: 47
- Joined: Tue Mar 12, 2013 8:50 am
Re: Carrs' Solder Stripper
I too have been wondering just what it was based on.
I even asked Hubert Carr about this a year or so ago but he explained he didn't know what it was formulated from as he simply acquired it from a manufacturer and rebottled it for modellers in smaller quantities.
The best info I managed to find was that it was possibly nitric acid based but no idea of percentages.
I've found it very useful but am now coming to the end of my last bottle. Not only will it eat solder but a brass assembly virtually disappeared after prolonged immersion. And anything steel causes much fizzing and eating!
I even asked Hubert Carr about this a year or so ago but he explained he didn't know what it was formulated from as he simply acquired it from a manufacturer and rebottled it for modellers in smaller quantities.
The best info I managed to find was that it was possibly nitric acid based but no idea of percentages.
I've found it very useful but am now coming to the end of my last bottle. Not only will it eat solder but a brass assembly virtually disappeared after prolonged immersion. And anything steel causes much fizzing and eating!
Last edited by decauville1126 on Fri Dec 30, 2016 9:55 am, edited 1 time in total.
-
- Posts: 381
- Joined: Mon Nov 23, 2009 9:22 pm
Re: Carrs' Solder Stripper
I do not recall ever selling this product in the four years I have been at C&L. We have safety data sheets for all the chemicals we currently use but I can find no reference as to the composition of solder stripper.
As the Company moved on from being a one man band to one with an employee base we had to take Health and Safety at Work on board and in particular the requirements of COSHH (Control of Substances Hazardous to Health). It is fair to say that a few of the substances which may have been sold in the past had such onerous levels of control requirements during the manufacturing process that we stopped producing them. Plastic Weld was one in particular which has not been available for several years. While it was 'safe' to use if the instructions on the bottle were followed (e.g. adequate ventilation) there was considerable risk involved in the bulk storage, handling and bottling process.
Roy
As the Company moved on from being a one man band to one with an employee base we had to take Health and Safety at Work on board and in particular the requirements of COSHH (Control of Substances Hazardous to Health). It is fair to say that a few of the substances which may have been sold in the past had such onerous levels of control requirements during the manufacturing process that we stopped producing them. Plastic Weld was one in particular which has not been available for several years. While it was 'safe' to use if the instructions on the bottle were followed (e.g. adequate ventilation) there was considerable risk involved in the bulk storage, handling and bottling process.
Roy
Return to “Product Information”